At what wire diameter should a compression spring be hot coiled instead of cold coiled?

The boundary is a section-size limit, not a preference. Cold coiling - winding at room temperature, then hardening and tempering - is normal up to about 10-12 mm carbon steel wire and to roughly 16 mm for chromium-silicon alloy wire. Above that the winding force, the springback and the quench section make hot coiling the practical route: the bar is heated above the austenitising range, wound, oil quenched and tempered.

The boundary is a section-size limit, not a preference. Cold coiling - winding at room temperature, then hardening and tempering - is normal up to about 10-12 mm carbon steel wire and to roughly 16 mm for chromium-silicon alloy wire. Above that the winding force, the springback and the quench section make hot coiling the practical route: the bar is heated above the austenitising range, wound, oil quenched and tempered.

What changes is the metal, not the drawing. Hot-coiled springs carry mill scale and a decarburised layer on the surface, and fatigue life follows the surface, so a cold-coiled spring keeps the wire it started with and takes a higher working stress. That is why a hot-coiled spring must be quoted with decarburisation measured and, on cyclic duty, peened to put compression back into the surface.

Tolerance is the second consequence. Cold coiling holds tighter dimensional control because there is no thermal growth or quench distortion to compensate; a hot-coiled heavy spring is set or ground to reach its free length. If your drawing demands a rate tolerance of a few per cent on a heavy spring, that is a cold-coiled or a set-and-ground part, and the price reflects it.

Two coiling routes for the same spring drawing
AspectCold coiledHot coiled
Practical wire rangeabout Ø1-12 mm carbon, to Ø16 mm alloyfrom about Ø12-16 mm upward, limited by heating and press capacity
Surface conditionwire surface retained, no oxide scalescale plus a decarburised layer that must be measured, ground or peened
Fatigue behaviourhigher working stress for the same lifelower working stress; peening recovers much of the difference
Dimensional controltight tolerance straight from the winderset or ground to length; more scatter as wound
Heat treatment routeaustenitise in a furnace after winding, oil quench, temperquench from the winding temperature, then temper
Typical productsdie springs, valve springs, machine springsground springs, large clutch and suspension springs, rail duty

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

The drawing says spring steel with no condition

A shop can coil almost anything and call the part finished. State the wire grade, the hardness after tempering, the permitted decarburisation depth and whether the spring is set, scragged or peened. Without those four lines the fatigue life of your spring is an assumption shared by everybody and owned by nobody.

You are copying an overseas heavy spring

The original may have been cold coiled from high-strength alloy wire while you hot coil the same dimensions from a cheaper grade: mass, rate and end condition then differ even though the drawing looks identical. Match by measured rate, stress and free length, and treat wire diameter alone as an insufficient specification.

Ground ends on a hot-coiled spring

Heavy springs are ground flat at the ends, which removes material exactly where the surface stress is highest and can leave a burned or locally softened layer if the grind is careless. Ask for hardness taken just under the ground surface on the sample, and set the grinding limits on the purchase order.

Questions buyers ask before they commit the specification

Why can a 25 mm wire spring not simply be cold coiled?

The winding force and the stored springback exceed ordinary mandrels, and a heavy section cannot be hardened uniformly afterwards, so the core stays soft and the rate is unpredictable. Hot coiling produces the part, but with the surface and tolerance penalties described above - which is why heavy springs are quoted with both routes considered.

Does decarburisation really matter on a spring?

Yes, more than on most parts. A decarburised surface layer holds less carbon, so it is weaker and carries less residual compression, and in a spring the maximum stress is exactly at the surface. Even a soft layer of a few tenths of a millimetre materially shortens fatigue life, so the depth is measured on a sample section.

Is peening worth paying for?

On cyclically loaded springs it usually is, because it puts compressive stress into the layer where cracks start. Specify intensity measured on standard strips, the media type and size, and the coverage required, and have the result recorded on the inspection sheet rather than asserted on the quotation.

Which route is cheaper at 14 mm wire?

Genuinely borderline, and the answer depends on the alloy, the shop tooling and your tolerance. We quote both routes with the tolerance and the life each one holds, and let the drawing decide, rather than picking one silently because the first quotation came back lower.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for springs repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationSprings category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.