Xingtai, Hebei · Hebei industrial clusters

Specification reference · updated 29 September 2026

Is Q355B the same as S355J2, and can A36 or SS400 replace it in a welded structure?

No. Q355B (GB/T 1591) and S355J2 (EN 10025-2) both guarantee 355 MPa minimum yield at 16 mm thickness, but Q355B is Charpy-impact tested only at +20 °C while S355J2 is tested at −20 °C. A36 (ASTM A36) guarantees 250 MPa yield, and SS400 (JIS G3101) is a tensile-based grade with no impact requirement, so neither is a like-for-like substitute in a loaded welded frame.

No. Q355B (GB/T 1591) and S355J2 (EN 10025-2) both guarantee 355 MPa minimum yield at 16 mm thickness, but Q355B is Charpy-impact tested only at +20 °C while S355J2 is tested at −20 °C. A36 (ASTM A36) guarantees 250 MPa yield, and SS400 (JIS G3101) is a tensile-based grade with no impact requirement, so neither is a like-for-like substitute in a loaded welded frame.

The substitution usually arrives as a price question: a mill offers A36 plate because it is on hand, cheaper and called equivalent. It is not. A member designed with a 355 MPa allowance loses roughly 30 % of its yield margin at 250 MPa, so the beam either deflects more or must be upsized - and the upsize changes connection details you already froze.

Impact testing is where the difference bites. EN grades carry a letter for the test temperature (J0 at 0 °C, J2 at −20 °C, K4 at −40 °C) and GB grades use the same logic (Q355B at +20 °C, C at 0 °C, D at −20 °C, E at −40 °C). For a cold site or a dynamically loaded member, the letter decides, not the number 355.

Structural steel grades - minimum values from the named standard, flat product up to 16 mm thickness
GradeStandardMin. yield Rp0.2 at 16 mmTensile RmCharpy V-notch requirement
Q355BGB/T 1591≥355 MPa450–630 MPa band, tabulated by thickness; certified value governs27 J minimum at +20 °C
Q355DGB/T 1591≥355 MPa450–630 MPa band, tabulated by thickness27 J minimum at −20 °C
S355J2EN 10025-2≥355 MPa450–600 MPa for 3–100 mm27 J minimum at −20 °C, longitudinal
S355J0EN 10025-2≥355 MPa450–600 MPa for 3–100 mm27 J minimum at 0 °C, longitudinal
A36ASTM A36/A36M≥250 MPa up to 100 mm thickness400–550 MPaNot specified by the grade
SS400JIS G3101not a yield-based grade; JIS gives an upper yield point by thickness band, about 245 MPa at 16 mm or thinner400–510 MPa above 16 mmNot specified by the grade

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

The drawing says S355 and the mill quotes Q355

Same 355 figure, different toughness letter, different carbon-equivalent ceiling and a different inspection document. A welding procedure qualified on EN plate does not automatically cover GB plate. Ask for the carbon equivalent, the impact test temperature and the certificate type before accepting the swap in writing.

The structure ships to a cold site or carries moving load

A36 and SS400 carry no impact criterion, so nothing in the grade proves the steel will not behave brittlely at a winter pour or a minus-20 °C design temperature. Where the code requires toughness, order S355J2 or Q355D and put the test temperature on the purchase order.

The part is machined, not welded

For a machined plate pocket, a base plate or a bracket blank, impact toughness is not the controlling property - flatness, thickness tolerance, machinability and internal stress are. There the A36-versus-S355 question becomes a documented cost decision rather than a structural one, and it should still be recorded on the drawing.

Questions buyers ask before they commit the specification

Can I substitute Q355B for S355J2?

For static load at ambient temperature it is often acceptable if the section is unchanged and your engineer signs the deviation. It is not acceptable for cold sites, dynamically loaded or fracture-critical members: S355J2 guarantees 27 J at −20 °C, Q355B only at +20 °C. The two also arrive with different inspection certificates, so check which document your designer needs.

Is A36 the same as Q235B?

They are close general-structural grades rather than identical ones. Q235B (GB/T 700) is a 235 MPa-class yield grade with a tensile band of roughly 370–500 MPa depending on thickness and a +20 °C impact requirement; A36 is 250 MPa yield with 400–550 MPa tensile and no impact requirement. Thickness bands and the impact criterion differ, so treat them as a designed substitution, not a free swap.

Does plate thickness change the grade?

Yes, and it is the most-missed line on an order. EN 10025-2 drops S355 from 355 MPa at 16 mm to 345 MPa for 16–40 mm, 335 MPa for 40–63 mm and 325 MPa for 63–80 mm, lower again in thicker bands. A36 falls to 220 MPa yield above 100 mm. Order 60 mm of S355 without re-reading the band and you lose design margin quietly.

What paperwork should arrive with the plate?

An EN 10204 3.1 certificate for export plate, naming grade and heat number and recording yield, tensile, elongation, impact values at the specified temperature and carbon equivalent, with the mill stamp on the plate matching the certificate. We cross-check heat numbers against the certificate at receipt and photograph the marking onto the inspection sheet.

Can you supply all four grades?

We buy to the grade your drawing names from plate and section mills in the Tangshan and Handan clusters, and we state on the quotation whenever a grade must be substituted, with the certificate of the replacement grade attached. We do not offer an unstated substitution, and we hold no mill authorisation - we are the purchasing and inspection team.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for steel products repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationSteel Products category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart