Xingtai, Hebei · Hebei industrial clusters

Specification references

The comparison tables we quote against

Every page here answers one substitution question with published standard values — grades, ISO dimension series, tolerance and clearance families, pressure-temperature bands — and says what breaks when the numbers are treated as interchangeable. Send the drawing and the same table comes back with your values in it.

34 references

Grouped by the category the decision belongs to

Written for the moment a buyer is handed a substitute and has to decide whether it is the same thing.

Which zinc coating protects my steel parts longest - electrodeposited, hot-dip galvanised or zinc flake?

Thickness decides it, and then the test endpoint. Zinc corrodes at a fairly steady rate in a given atmosphere, so 8 µm of electrodeposited zinc is not a thin version of a 70 µm hot-dip coating - it is roughly a decade less life. ISO 1461 tabulates hot-dip minimum thickness by base-material thickness, and ISO 9227 salt-spray hours measure something different from outdoor service because the chamber never dries.

Open the comparison table →

Should this part be forged or cast - and how do volume, mechanical properties and defect risk decide?

By geometry and volume first, load path second. Casting buys shape: internal cavities and complex bosses from one pour, and it tolerates a thick-to-thin transition a die cannot fill. Forging buys soundness and direction: closed grain flow following the load and more fatigue margin per kilogram. At one-off to low hundreds a pattern is cheap and a forging die is not; at tens of thousands it reverses.

Open the comparison table →

Do I need a P6 or P5 bearing, or is normal-class P0 good enough?

P0 unless something in the machine says otherwise. ISO 492 classes tighten dimensional and running accuracy - mean bore and outside-diameter deviation, width variation, ring runout - and they raise nothing else. A P5 bearing with the same designation is the same rolling geometry in a narrower tolerance band, so the money buys fit control, speed behaviour and radial runout, not load capacity or fatigue life.

Open the comparison table →

How is a hydraulic rod-seal gland designed, and which standard fixes the grooves for the seal, the wiper and the back-up ring?

The gland is a machined interface with its own standards, not part of the seal catalogue. ISO 10294-3 and ISO 10294-4 publish groove dimensions and tolerances for general-duty and heavy-duty reciprocating rod seals, ISO 6194 covers wiper rings, ISO 7795 covers back-up rings used with elastomer rings, and ISO 5597 fixes the preferred bore and rod diameters every one of those tables is indexed against.

Open the comparison table →

Which hydraulic cylinder mounting style do I need, and what do the mounting codes actually change?

The mounting decides three things before the bore does: where the reaction load enters the machine, how much side load the rod sees, and how much misalignment the joint absorbs. Foot and flange mountings - the metric families of ISO 6020-1 and ISO 6020-2 - are rigid and demand alignment. Eye, clevis and trunnion mountings pivot, so they self-align but load a pin that must be sized for it.

Open the comparison table →

What is the difference between RF, FF and RTJ flange faces, and which pressure class needs which?

The facing decides where the gasket sits. A raised face (RF) puts an annular ridge inside the bolt circle so a ring gasket is compressed and contained; a flat face (FF) seals across the whole annulus and is used where the mating flange is unreinforced, typically cast iron equipment; a ring joint (RTJ) machines a groove for a metal ring and is chosen for high pressure and high temperature.

Open the comparison table →

At what wire diameter should a compression spring be hot coiled instead of cold coiled?

The boundary is a section-size limit, not a preference. Cold coiling - winding at room temperature, then hardening and tempering - is normal up to about 10-12 mm carbon steel wire and to roughly 16 mm for chromium-silicon alloy wire. Above that the winding force, the springback and the quench section make hot coiling the practical route: the bar is heated above the austenitising range, wound, oil quenched and tempered.

Open the comparison table →

Which cast valve body material suits PN10, PN16 or PN25, and why does the same PN derate with temperature?

PN is not one number: it is a pressure at 20 °C, and every material loses allowable pressure as the fluid gets hotter. Grey cast iron (EN-GJL-250) holds PN16 at ambient but derates steeply above about 100 °C, ductile iron (EN-GJS-400-15) holds PN16 further up the scale, cast carbon steel and cast stainless further again. Read the pressure-temperature table for the material group, not the nameplate.

Open the comparison table →

Will an ISO 7241-A coupling mate with a B, and when should a flat-face coupling be used instead?

No, and the two letters are worth learning. ISO 7241-1 covers interchangeable bullet-valve couplings with a ball lock, in Series 1 (A) and Series 2 (B); their shells and locking geometry differ, so halves of the two series engage far enough to look compatible and then leak, jam or damage the valves. Flat-face couplings are a separate family, dimensioned by ISO 7241-2 and by ISO 16028.

Open the comparison table →

Is hard anodising (Type III) worth specifying over standard Type II on an aluminium part?

When wear is the problem, not weather. Type II is the ordinary sulfuric anodic coating, typically 5-25 µm, takes dye well and is the standard answer for appearance and general protection. Type III is the hard-coat family: dense, commonly 25-75 µm, markedly harder, chosen for abrasion, galling and dielectric duty - and it takes colour badly. The thickness range is the specification; the type word alone is not one.

Open the comparison table →

Is 70 Shore A the right hardness for my part, and what does the durometer number not tell me?

Hardness measures resistance to an indenter, not strength. ISO 48-4 covers the durometer method, and the practical rule is that readings above about 90 on the A scale lose reliability, so hard compounds are measured on the D scale. Two parts reading 70 Shore A can behave quite differently, because tensile strength, modulus and compression set come from the polymer and the cure, not the durometer.

Open the comparison table →

Written first reply within 1 working day; priced answer within 2-5 working days.

Specification not covered here?

Send the standard your engineer named, the drawing and the quantity. We answer with the comparison, the substitution we recommend and the inspection plan that proves it.