Xingtai, Hebei · Hebei industrial clusters

Specification reference · updated 29 September 2026

Which conveyor belt cover class and splice method should I specify for my material?

Cover grade and joint method are one decision, not two. The cover takes the impact and the abrasion; the splice carries the tension, and a splice can only keep the share of belt strength its method allows. A hot vulcanised joint approaches full carcass strength, a cold adhesive joint keeps a smaller share, and a mechanical fastener typically keeps well under half.

Cover grade and joint method are one decision, not two. The cover takes the impact and the abrasion; the splice carries the tension, and a splice can only keep the share of belt strength its method allows. A hot vulcanised joint approaches full carcass strength, a cold adhesive joint keeps a smaller share, and a mechanical fastener typically keeps well under half.

Belts are designated by carcass and strength, in the common form EP 400/4 10+3: EP for the polyester fabric carcass, 400 for tensile strength in newtons per millimetre of width, 4 for the number of plies, and 10 and 3 mm for the top and underside cover thickness. Steel cord belts are designated by cord strength and are spliced by vulcanising to the maker tables only.

Cover rubber is chosen by what it carries: abrasion, load temperature, oil or fat in the stream, and whether the site demands fire resistance. Those are compound decisions with test methods behind them - the standard abrasion volume-loss test, immersion volume change to ISO 1817, and the fire and surface-resistance tests that underground duty requires. Material and belt dimensions sit in EN ISO 14890.

Splice methods and the belt strength each one keeps
Splice methodShare of tensile strength keptWhat it needs on siteWhere it is the wrong answer
Hot vulcanised (press)approaches the full carcass strength when correctly madeskived step joint, press at the stated temperature, pressure and time, controlled coolingshort shutdown windows, and steel cord joints made without the maker tables
Cold vulcanised (room-temperature adhesive)a substantial but lower share, wholly dependent on surface preparationbuffed rubber and fabric, primer, full clamp pressure across the overlap, minimum cure temperaturehot, wet or oil-washed joints and long high-tension conveyors
Hinged mechanical fastenerstypically well under halfbelt thickness inside the fastener range and the correct punch pitchsteep inclines, high tension, transfer points and pulley nips
Bolted clamp lacingthe lowest share, and a permanent wear pointa clean cut edge and regular re-tensioningcontinuous-duty plants and any long route
Steel cord splicefull strength only as a vulcanised stepped splicethe maker splice table, cord spacing and cover build-upnever with mechanical fasteners

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

Cover thickness bought from the cheapest line

A thinner top cover costs less per metre and fails sooner, and the minimum cover values in the belt designation exist because impact and abrasion remove rubber at a predictable rate. Choose the top cover from lump size, drop height and throughput, then let the price fall out of that decision rather than the reverse.

The joint is the belt real strength

A 630 N/mm belt finished with a mechanical fastener behaves as a much weaker belt with an expensive carcass inside it. Specify the splice method in the purchase order, who makes it, and with what equipment, because the joint is where the maintenance manager will look first when the line stops.

Heat, oil and impact each rule a compound out

A general-purpose cover softens and loses volume as load temperature climbs, an oil-wetted stream swells standard rubber, and hot sinter blisters a cover that was never rated for it. Ask for the compound class and the measured test values rather than an adjective on a datasheet.

Questions buyers ask before they commit the specification

Which belt lasts longest in a quarry?

The one matched to the actual load temperature, lump size, drop height and pulley diameters. Abrasion resistance alone is not the answer, because a very hard cover tears under large impact and a soft one wears away. Send the material data and the routing and we quote against both.

Can an existing belt be extended?

With a matched splice, yes: the new roll should share the designation family, the cover class and a compatible thickness so the skived steps line up. Mixing carcass types is a maintenance shortcut that shows up as a joint failure inside the first month of running.

What belt data do you need to quote?

Declared tensile strength and plies, cover class and thickness, minimum pulley diameter, fire class if the route is underground, the joint method and the length. We return the splice plan with the shipment paperwork so the site crew is not improvising at the joint.

Can you supply the fasteners and punch too?

Yes, as a controlled accessory with the correct punch and the belt thickness range stated, because a mismatched fastener is the commonest reason a quickly made joint fails slowly and expensively, and it is cheap to prevent on the order.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for conveyor belting & rubber sheets repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationConveyor Belting & Rubber Sheets category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.