Xingtai, Hebei · Hebei industrial clusters

Specification reference · updated 29 September 2026

Which EN 10213 cast steel keeps its toughness at a sub-zero design temperature?

None of them automatically. In EN 10213 the family and chemistry make an answer possible; the Charpy V-notch test temperature is a condition you write into the order. A valve body or pump casing specified only as cast steel can arrive with toughness proven at +20 °C and then behave in a winter commissioning test exactly like the specification did not require.

None of them automatically. In EN 10213 the family and chemistry make an answer possible; the Charpy V-notch test temperature is a condition you write into the order. A valve body or pump casing specified only as cast steel can arrive with toughness proven at +20 °C and then behave in a winter commissioning test exactly like the specification did not require.

Read the designation as three decisions. The non-alloy and lightly alloyed weldable cast steels - the general-pressure family, where a figure such as 240 names a minimum yield for a stated thickness band - are the ordinary ambient answer. The low-alloy chromium-molybdenum grades, quenched and tempered, buy strength and elevated-temperature behaviour. The austenitic and duplex cast stainless families keep working where a ferritic steel cannot be qualified, because face-centred-cubic iron has no ductile-to-brittle transition to fall off.

What must be contracted is the test: temperature, energy, and whether acceptance is an average or an individual value. Heat treatment belongs in the same order, because a toughness claim about a casting that was not heat-treated as the grade requires is a claim about a coupon, not about your part. Section is the last constraint - a 90 mm boss cannot be through-hardened like a 20 mm wall, which is why the standard tabulates by thickness band.

EN 10213 families and how low-temperature capability is actually contracted; strength and impact values are tabulated by thickness band and heat treatment - confirm the band for your wall on the certificate
Family and example designationMetallurgyWhat the standard asks forLow-temperature pictureTypical part
CS general-pressure non-alloy weldable cast steel (GP 240 GH type)carbon cast steel, weldable with a qualified procedureyield and tensile minima by thickness band, plus impact at the temperature stated in the orderthe ordinary default is tested at +20 °C; anything lower is an added condition, not impliedpump and valve bodies, pressure housings, gear cases at ambient
CS slightly alloyed weldable (G 235 Cr type)non-alloy to low-alloy, normalised conditiontensile band and hardness limits by sectionsame logic: the test temperature is written by the buyerhousings and frames where welding and machining lead
LS low-alloy specified-property grades (G 20 Cr Mo 5 type)about 1 % Cr - 0.5 % Mo, normally quenched and tempereda hardness or tensile window for the condition, with impact at the contracted temperaturecapable of sub-zero testing when the heat treatment and the test are ordered togetherloaded hubs, high-pressure bodies, gear and pinion blanks
LT orders with defined low-temperature toughnessnickel-alloyed or carefully heat-treated ferritic gradesCharpy V-notch energy at 0, -20, -40 or -60 °C as specifiedthis is the family you name when the design temperature is below freezingrefrigeration, cold-region and LNG-adjacent pressure parts
Austenitic cast stainless - 1.4308 and 1.4408 typesCr-Ni and Cr-Ni-Mo, face-centred cubictheir own strength band, with impact usually agreed rather than transition-limitedthe practical answer well below what ferritic cast steel can be qualified for, down to cryogenic serviceseawater, chemical and cryogenic housings and valve bodies
Ferritic-austenitic (duplex) cast - 1.4462-type chemistryduplex Cr-Ni-Mo-Na higher strength band than the austenitic grades with agreed impact valuestough at moderately low temperature and strong against chloride, within the process standard temperature limitspressure parts in chloride and seawater duty

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

The pattern carries a grade and the order carries no test temperature

The foundry delivers the minimum the standard requires and the certificate is lawful. What is missing is the toughness the site needs. Design temperature, minimum ambient during commissioning, and the required energy with its test temperature belong on the purchase order, together with the acceptance rule for individual and average values.

A weld repair on a tested casting

Local welding alters the condition that the impact test represented, and on low-alloy quenched-and-tempered material it can leave a soft or hard zone that the original certificate says nothing about. Agree the repair procedure, whether the part is re-heat-treated, and whether the affected area is re-tested before the casting is accepted.

A thick section that cannot be hardened as the grade assumes

Quenched-and-tempered properties depend on cooling rate, so a heavy boss and a thin wall from the same pour are not the same material. Ask what the actual section is at the loaded features, take hardness on the body where the standard allows, and let the certificate name the thickness band the values were taken from.

Questions buyers ask before they commit the specification

Can a cast steel body be used at minus 40 °C?

Yes, by choosing the family and contracting the test. Either a ferritic grade qualified by Charpy at that temperature - usually a nickel-alloyed or carefully heat-treated one - or an austenitic cast stainless, which has no transition to worry about. What does not work is ordering the ambient grade and hoping the impact figures transfer from the low-temperature catalogue line.

Is EN-GJS-400-18-LT ductile iron an alternative to cast steel for cold service?

Sometimes, and it is worth pricing both. The -LT ductile iron designation exists precisely to carry a Charpy requirement at minus 20 °C, and it casts and machines more cheaply than steel. The deciding factors are the pressure and temperature the design code allows, the section, and whether the part is welded - where cast steel generally has the better record.

What certificate should a pressure casting arrive with?

An EN 10204 3.1 document naming the grade and heat treatment, the thickness band the values were taken from, chemistry, tensile, hardness and the Charpy results with their test temperature and specimen location, plus the NDT method and acceptance class. For pressure equipment the notification body and material approval trail are a separate question, and the certificate type is decided before the pattern is made.

Which non-destructive tests actually matter here?

Volumetric inspection first, because castings fail inside: radiography to ISO 4993 for steel castings or ultrasonic testing to the EN 12680 acceptance classes, chosen against the wall thickness you can actually shoot through. Magnetic particle testing to ISO 9945 and penetrant testing to ISO 12706 find the surface-connected defects - and both belong on the drawing with an acceptance level, not in a conversation.

Can you replace an obsolete casting mark from an old machine?

Usually, working from what the part has to carry rather than from the letters on it: strength band, toughness at a temperature, chemistry, section, and the code the component is designed to. We return a named grade with the values beside the old mark, and the deviation goes to your engineer for written approval before anything is tooled.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for iron & steel castings repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationIron & Steel Castings category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.