Xingtai, Hebei · Hebei industrial clusters

Specification reference · updated 29 September 2026

Is EN-GJS-500-7 the same as A536 65-45-12, and which ductile iron grade should the casting be ordered to?

Not directly, and the trap is units. A536 names its three figures in ksi, so 65-45-12 means 65 ksi minimum tensile - about 448 MPa - while EN 1563 names megapascals, so EN-GJS-500-7 is 500 MPa. A cross-reference that pairs the two without saying one is 448 MPa and the other 500 MPa quietly hands you a weaker part or a heavier one.

Not directly, and the trap is units. A536 names its three figures in ksi, so 65-45-12 means 65 ksi minimum tensile - about 448 MPa - while EN 1563 names megapascals, so EN-GJS-500-7 is 500 MPa. A cross-reference that pairs the two without saying one is 448 MPa and the other 500 MPa quietly hands you a weaker part or a heavier one.

The second axis is the microstructure the numbers come from. The elongation figure is really the ferrite report: 400-15 and 400-18 are ferritic, formable, machinable and the toughest of the group, while 600-3 and 700-2 are pearlitic or specially treated, harder, stronger and far less willing to bend. That is why a grade swap for "more strength" can turn a weld, a bolted flange or a shock load into a crack.

The third axis is section. Both standards tabulate their minima by wall thickness, because a thick pour cools slowly, grows fewer and larger nodules, and loses elongation. Order a heavy 400-15 flange against the 20 mm column and the certificate will not match the drawing. Name the band, say whether the test bar is separately cast or taken from the body, and put a hardness check on the order too.

EN 1563 spheroidal graphite cast irons with their usual A536 neighbours - minima for the standard thickness band; confirm the band that fits your wall from the standard and the certificate
EN 1563 gradeMin. tensileMin. yield Rp0.2Min. elongationNearest A536 grade (ksi)What the numbers mean
EN-GJS-400-15400 MPa250 MPa15 %60-40-18 (414 MPa)ferritic: formable, machinable, weldable with care, the choice where the part must bend or be repaired
EN-GJS-400-18-LT400 MPa240 MPa18 %no clean A536 twinthe low-temperature member of the family, with a Charpy requirement at minus 20 °C written into the designation
EN-GJS-500-7500 MPa320 MPa7 %80-55-06 (552 MPa)ferrite-pearlite balance: the general structural compromise for housings, hubs and brackets
EN-GJS-600-3600 MPa370 MPa3 %100-70-03 (690 MPa)mainly pearlitic: harder faces, wear contact, crank and gear blanks; limited forming
EN-GJS-700-2700 MPa410 MPa2 %120-90-02 (827 MPa)high-strength pearlitic or treated condition, and the point where the A536 names start to overshoot the EN figures
EN-GJS-800-2 (austempered practice)800 MPa480 MPa2 %above the ordinary A536 listaustempered (ADI) route: very high strength with useful toughness, but it needs a heat treatment the whole order must be written around

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

The drawing is in EN, the pattern shop works to ASTM

Someone reads "65-45" as "roughly 500" because both numbers appear in the same column of a chart. Send the MPa figures, the required hardness band and the test method with the enquiry, and let the foundry confirm which grade and which thickness band carries them. A grade named across two systems without the numbers is a grade nobody has ordered.

A 400-15 is swapped to 500-7 for a stronger boss

You gain tensile and lose the elongation and the ferrite that let the part absorb a knock, flex at the mounting feet or survive a local weld repair. Where the real problem was a thin section or a stress riser, the higher grade makes it brittle rather than fixing it. Ask for the geometry change and the grade change as two separate questions.

The certificate tests a separately cast bar, not your casting

That is the normal EN 1563 arrangement, and it proves the pour, not the core of a 60 mm boss. Where the part is structural or pressure-retaining, ask for hardness on the body, a metallographic check of nodularity and ferrite where agreed, and volumetric inspection to a stated acceptance class - and put the level of soundness on the drawing before the pattern is cut.

Questions buyers ask before they commit the specification

Which grade is right for a pressure-retaining housing?

Usually one of the ferritic or mixed grades - 400-15 or 500-7 - because the deciding factor is soundness and machining stock rather than tensile class. A leak-tested housing fails at shrinkage porosity and inclusions, not at the grade number. Specify the proof pressure, the inspection method and its acceptance class, and let the strength grade follow the structural load.

Is ductile iron weldable?

Weldable with a qualified procedure, and the ferritic grades are the forgiving ones. Common practice is preheat on thicker sections, nickel-type or matching flux-cored consumables, controlled interpass temperature and slow cooling, and machining or grinding after rather than before. Expect a hard, unmachinable white zone at the fusion line unless the procedure includes the post-weld thermal step.

Does a higher grade mean better wear resistance?

Only mildly. 600-3 and 700-2 run harder and hold abrasive contact better than 400-15, but genuine abrasion is a different material question: white irons and chrome-alloyed irons, or a hardened overlay, are what mining and aggregate duty is built from. Choosing 700-2 for slurry wear buys strength you did not need and still wears out.

What paperwork should arrive with the castings?

An EN 10204 3.1 certificate naming grade, pattern or heat, the thickness band tested, tensile, yield, elongation and hardness, and the impact figures where a -LT grade was ordered. Add the dimensional report, the NDT method and acceptance class, the modification or inoculation record if the foundry works to it, and the heat-treatment chart for austempered or quenched-and-tempered conditions.

Can you supply both standards, and how do you decide?

We quote either against the numbers on your drawing rather than the grade word, and we show the comparison when the drawing names one system and the market stocks the other. Where a substitution is cheaper or faster, it goes to you as a written deviation with the mechanical values beside the original, and nothing is changed silently. We are the buying and inspection desk, not the foundry.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for iron & steel castings repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationIron & Steel Castings category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart