What makes a high-strength structural bolt different, and how is a wedge load test actually performed?

A structural high-strength bolt is sold as a system, not as a screw. EN 14399 supplies bolt, nut and washers as one set with a declared friction coefficient and a required pretension, and the joint is designed to carry load by friction between the faying surfaces. An ordinary class 10.9 bolt tightened to a torque value is a fastener, not a bolting system.

A structural high-strength bolt is sold as a system, not as a screw. EN 14399 supplies bolt, nut and washers as one set with a declared friction coefficient and a required pretension, and the joint is designed to carry load by friction between the faying surfaces. An ordinary class 10.9 bolt tightened to a torque value is a fastener, not a bolting system.

The two main families are HV, a large hexagon head used with hardened washers, and HR, a countersunk head used where the surface must stay flush. Designations such as HV6, HV10, HR6 and HR10 differ in head form, size range and tightening-control method, and the pretension values are tabulated by diameter in the relevant part of the standard.

The wedge load test is how the head and thread are proved rather than the shank. The bolt is pulled with a hardened wedge under its head; the fracture must occur in the shank or with at least one engaged thread past the nut face. A head or fillet failure means the fillet radius, the forging or the heat treatment has a problem, whichever class was ordered.

What each test and requirement actually proves
Test or requirementWhat it provesGoverning documentHow we verify at receipt
Wedge tensile (wedge load) testHead, fillet and thread in the real load pathISO 898-1 for property classesCertificate plus a sampled pull test on the lot
Hardened wedge under the headForces failure away from the anvil so a weak fillet cannot be maskedISO 898-1 test methodPhotograph of the rig and the fracture in the report
Tensile Rm and yield Rp0.2The material class of the bolt itselfISO 898-1, EN 14399Head markings cross-checked against the certificate
Rotational capacity testThe nut and washer do not seize before the bolt yieldsEN 14399 parts for the system orderedRequested and recorded on preloaded orders
Pretension and control methodThe friction grip actually forms in the jointEN 14399 with the design rules of EN 1993-1-8Tightening instruction in the shipment file
Declared slip factorThe faying surface condition you may design forEN 1993-1-8, verified on siteBlast profile and test report on file

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

Your engineer writes M20 10.9 but the joint is slip-critical

That is a category error rather than a price question. A slip-critical joint needs a bolting system with washers, a defined preload and a method of achieving it, because the design assumes the clamp force exists. We flag it in writing on the quotation instead of quietly shipping the cheaper reading of the bill of materials.

Re-using a pretensioned bolt

A preloaded HV or HR bolt that has been tightened into its yield range is generally not re-used, and re-using the washers changes the nut factor that the tightening procedure was built around. If the design permits re-use, that permission has to be stated and verified rather than assumed by the crew on site.

Coating and class must be decided together

Galvanised high-strength sets carry a hydrogen risk that needs a post-plating bake, and a lubricated thread changes the torque-to-preload relationship, which changes the tightening instruction the site uses. Never re-lubricate or re-coat a set without issuing a new tightening procedure with it.

Questions buyers ask before they commit the specification

Is a wedge test the same as a plain tensile test?

No. Under plain tension the head can support the bolt and hide a weak head-to-shank fillet. The wedge puts a defined angular bearing under the head so the failure reveals whether that region is adequate, which is why the method is specified for hexagon bolts and screws rather than left to a shop choice.

What is the difference between HV and HR bolting?

HV is a large hexagon head set used with hardened washers. HR is a countersunk head set used where the surface must remain flush, for example plate edges and moving structures. Both are controlled-tightening systems supplied with their washers, and both are covered by separate parts of EN 14399.

Where do I find the pretension values to apply?

In the EN 14399 part covering your bolting system, by diameter, and in the design code EN 1993-1-8 for what proportion of proof load the joint design uses. In North American practice the equivalent figures come from the structural bolting installation specification with ASTM F3125 A325 and A490 installation tension.

Can you supply the washers separately to save cost?

The set is the item. A bolt, nut and washer assembled from three suppliers has unverified friction behaviour, and the rotational capacity and slip-factor claims no longer hold. We buy sets, record the declared friction coefficient and keep the certification with the shipment documents.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for fasteners & bolts repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationFasteners & Bolts category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.