Xingtai, Hebei · Hebei industrial clusters

Specification reference · updated 29 September 2026

Which elastomer resists which fluid - nitrile, EPDM, HNBR, FKM or FFKM?

There is no general best compound, only the right one for the medium and the temperature. NBR is the oil and fuel workhorse and it fails in steam and ozone. EPDM is the opposite: steam, hot water and glycol brake fluid, destroyed by mineral oil. FKM covers fuels, aromatics and hot oils but is attacked by steam, ketones and amines. FFKM is the last resort when everything else swells.

There is no general best compound, only the right one for the medium and the temperature. NBR is the oil and fuel workhorse and it fails in steam and ozone. EPDM is the opposite: steam, hot water and glycol brake fluid, destroyed by mineral oil. FKM covers fuels, aromatics and hot oils but is attacked by steam, ketones and amines. FFKM is the last resort when everything else swells.

Read the test rather than the claim. Compound resistance is published as volume change and hardness change after immersion to ISO 1817 at a stated temperature and exposure time, and the figures that matter are swell, extraction and the loss of tensile and elongation. A compound that looks identical on a summary chart can pass at 40 °C for 70 hours and fail at 100 °C.

Nitrile itself has a dial. Acrylonitrile content in NBR runs roughly 18 to 42 %, and more acrylonitrile means better resistance to aromatic fuel and oil but worse flexibility in the cold. That is why two parts both described as 70 Shore A nitrile behave very differently in an outdoor hydraulic unit at -25 °C.

Media and temperature picture by elastomer family (ISO 1629 nomenclature)
ElastomerContinuous temperatureGood againstAvoidTypical hardness
NBR nitrile-30 to +100 °Cmineral oil, hydraulic fluid, grease, dieselsteam, ozone, glycol brake fluid, ketones50-90 Shore A
HNBR hydrogenated nitrile-40 to +150 °Chot oil, ozone, dynamic load, belts and rod sealsstrong acids, polar solvents60-90 Shore A
EPDM-40 to +150 °C (short 175 °C)steam, hot water, glycol fluids, ozone, weatheringmineral oil, fuel, aromatic solvents50-90 Shore A
VMQ silicone-60 to +200 °Ccold flexibility, weathering, wide temperature bandabrasion, pressurised steam, fuels and oils40-80 Shore A
FKM fluoroelastomer-20 to +200 °C (grades to -30 °C)ethanol-blended fuel, aromatics, hot oilsteam, ketones, amines60-90 Shore A
FFKM perfluoroelastomer-15 to +250 °Caggressive chemical and solvent mixturescost; some amines and steam regimes still bite65-95 Shore A

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

The compound is quoted without the cure system

Peroxide-cured nitrile holds heat and compression set far better than standard nitrile cured the conventional way. Two parts on a drawing both described as NBR 70 Shore A can therefore be some tens of degrees apart in real service, and the cheaper one is the one that leaks first in the hot zone.

Intermittent heat is worse than steady heat

A seal that survives a steady 100 °C can still fail the cycling, because compression set accumulates and the relaxing ring loses its sealing force between cycles. State the cycle count and the dwell at temperature in the enquiry, not only the peak figure the machine can reach.

Moulding history is part of the specification

Post-cure, release-agent choice and tooling cleanliness all change a moulded surface, and a ring moulded in tooling used for a waxing compound can arrive with a film that leaks at first assembly. We ask for the compound lot and the post-cure condition and record both with the shipment.

Questions buyers ask before they commit the specification

Which elastomer for a brake system?

EPDM, because glycol-based brake fluid and the temperature swing behind a hot hub suit it while nitrile swells. Check the whole circuit before assuming: some clutch and hydraulic lines on the same vehicle run mineral oil, where EPDM is the wrong answer and NBR or HNBR is right.

Which one for diesel with ethanol blended in?

FKM handles ethanol-blended diesel far better than standard NBR, which can swell and soften, with HNBR sitting between the two for lower-cost duty. Choose against the actual blend percentage and the temperature the seal sees, and ask for the immersion test data behind the recommendation.

Is FFKM always the safe choice?

It has the broadest chemical coverage and the highest temperature range, but it costs an order of magnitude more and is not automatically better mechanically, and some amine and aggressive mixtures still attack it. Specify it against the immersion data for your medium, not against general worry.

How do you verify a compound after delivery?

Hardness, density, tensile and elongation against the compound datasheet, with the lot code kept on the packing list so a part traces to its batch. Where the duty is critical we arrange independent compound identification, and its report is passed on with the shipment documents.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for rubber & plastic parts repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationRubber & Plastic Parts category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.