Is 70 Shore A the right hardness for my part, and what does the durometer number not tell me?

Hardness measures resistance to an indenter, not strength. ISO 48-4 covers the durometer method, and the practical rule is that readings above about 90 on the A scale lose reliability, so hard compounds are measured on the D scale. Two parts reading 70 Shore A can behave quite differently, because tensile strength, modulus and compression set come from the polymer and the cure, not the durometer.

Hardness measures resistance to an indenter, not strength. ISO 48-4 covers the durometer method, and the practical rule is that readings above about 90 on the A scale lose reliability, so hard compounds are measured on the D scale. Two parts reading 70 Shore A can behave quite differently, because tensile strength, modulus and compression set come from the polymer and the cure, not the durometer.

The bands are still useful. Very soft compounds around 30-40 A conform to irregular surfaces; 50-60 A covers grips, diaphragms and low-pressure seals; 70 A is the industry default because it balances contact stress against extrusion; 80-90 A takes higher static load and resists abrasion better, at the cost of friction and heat in dynamic duty. Above that you are approaching hard rubber, where an A reading is the wrong instrument.

Two measurement facts decide what the number means. The specimen must be thick enough that the indenter does not feel the anvil - about 6 mm minimum for the A scale, with thin parts stacked - and the reading depends on when it is taken, because rubber relaxes under the foot. Then the compound: 80 A nitrile, 80 A fluorocarbon and 80 A polyurethane are three prices, three abrasion lives and three low-temperature behaviours at one hardness.

Durometer bands and what each one is chosen for - the compound family, the cure and the geometry still decide performance, and the measurement conditions belong on the inspection record
Hardness bandTypical applicationWhat you are really buyingWhat it does not buyMeasurement note
30-40 Shore Adamping pads, soft seals on rough or out-of-round surfaces, protective bumpersconformability and low contact stressresistance to extrusion under pressure, and abrasion lifevery soft materials relax quickly; state the reading time and use the correct foot
50-60 Shore Agrips, bellows and diaphragms, low-pressure sealing, flexible sheeta balance of flex and durabilityload capacity in compression and cut growth resistancesoft grades take a permanent set under sustained load; ask for compression set
70 Shore Athe default for moulded seals and O-rings, feet, general bushingsthe sealing compromise the market stocks and pricesany medium resistance at all - that is the polymer family, not the hardnessmeasure on a bulk specimen; a moulded skin reads differently from the section
80 Shore Aloaded bushings, wheels and castors, wear strips, buffersless deformation under load than 70 A, better abrasion behavioursealing on a poor surface, and low friction in reciprocating dutythick sections cure with a gradient, so check the core as well as the surface
90 Shore Aheavy buffers, coupling elements, high-wear partsthe top of the practical A-scale rangeplastic-like rigidity; and where 90 A is being chosen to stop extrusion, the clearance and a back-up ring are the real answerat this end, verify the scale and the spring force used - readings scatter
Above 90 A, measured on Shore Dhard rubber, ebonite-type compounds, rigid industrial profilesa valid number from a different indenter and springany comparison with an A reading without an approximation table, which is not exactstate the scale on the drawing; "95" with no scale is not a specification

Values are the published minima, maxima or bands of the standards named in the table, taken at the stated thickness, size or temperature. Where a standard tabulates a value by size band, the value for your goods comes from the mill or test certificate, which we attach to the quotation instead of summarising it here.

Where this costs money

Three situations where the difference becomes a claim

Each is a decision taken at quotation stage, while the specification is still cheap to change.

A purchase order that says only "rubber, 70 degrees"

No scale, no method, no compound, no medium, no temperature. Three suppliers will answer with nitrile, EPDM and a recycling-loaded compound of the same hardness and the same colour, and only one of them will survive the oil. Write the ISO 1629 compound family, the hardness with its scale and tolerance, and the service conditions - the durometer is one line of a specification, not the specification.

Hardness raised to stop a leaking seal

A harder ring needs more squeeze to seal, transmits more wear to the rod, follows surface waviness less well and extrudes into the same clearance at the same pressure. Where the problem is the gap, the answer is the clearance, a back-up ring or the gland finish, and a hardness increase buys friction and heat instead of a seal.

The same hardness in a different polymer

At 80 A, polyester and polyether polyurethane beat most rubbers on abrasion, fluorocarbon wins on hot fuel and loses on cold flexibility and price, and EPDM refuses mineral oil entirely. Choosing by durometer alone is how a part that is nominally identical fails on the second week of service, which is a compound decision the enquiry has to force.

Questions buyers ask before they commit the specification

Is there a conversion table between Shore A and Shore D?

Approximate comparison charts exist and they are only that. The two scales use different indenters and spring forces, and a viscoelastic material responds differently to each, so a converted figure proves nothing on its own. Specify the scale the material is actually controlled on and measure on it - for a compound that reads near the top of the A range, quote D.

Does hardness tell me how much load the part carries?

Not on its own. The stiffness of a rubber mount is a function of modulus, shape factor and bonded area as much as durometer, and long-term load retention is compression set rather than initial hardness. Where a spring rate or a deflection is the requirement, ask for the load-deflection curve for that geometry and the compression set figure at the service temperature.

How do you check hardness on delivered parts?

With a calibrated durometer on a specimen of adequate thickness - stacking thin pieces where necessary - at controlled temperature, at a stated time after the foot lands, taking several readings per part and per mould cavity. We record the scale, the specimen condition and the values rather than writing "70 Shore" onto the inspection sheet, because that is the only version of the number that is repeatable.

Why is my thick moulded part soft at the surface?

Thick sections cure with a gradient, and over-cure can revert the network, leaving a softer skin or an under-cured core while the outside reads correctly. It shows up as inconsistent compression set rather than as a hardness failure. Ask for cure evidence and a section check on the trial parts, and measure the core on a cut face when the geometry is beyond the moulding shop normal.

Do you buy to hardness or to compound?

To a compound family with a declared hardness band, matched to the medium, the temperature range and the dynamic or static duty. The quotation names the ISO 1629 code, the band with its scale, and the tests we will run; and where a cheaper compound at the same durometer is proposed, that is written as a deviation with the reason, so nobody discovers the difference in service.

Fit this to a real part

Send the drawing and the answer comes back with your numbers

The quotation for engineering rubber repeats this comparison against your grade, dimension, tolerance and test package, and names any deviation before production starts.

Ask about this specificationEngineering Rubber category hub

How we verify it

  • Grade and condition checked against the EN 10204 3.1 certificate and the heat marking.
  • Boundary dimensions, class, clearance or rating measured on the inspection sheet.
  • Deviations offered in writing before production, never discovered after shipment.

Trading and sourcing company based in northern Xingtai, Hebei, about 60 km south of the provincial capital. We buy across the industrial clusters of central and southern Hebei and reach the northern ones on scheduled factory runs; the supplier visits, benchmarking and pre-shipment inspection are ours, done in person. Not a factory. Multi-category, quoted from drawings, consolidated into one container and one document pack, and inspected before the balance is paid; every order starts as an RFQ.

Inspection and documents →

Written first reply within 1 working day; priced answer within 2-5 working days.

Quote it against your part, not the chart

Send the drawing, the standard your engineer named and the quantity. We reply with the priced specification, the substitution we recommend and why, and the inspection plan that proves it.